When using accelerator (hot processing)
- Temperature (min. 80 +/- 5 °C) of cartridge oven must be checked every morning. Connect temperature sensor to DIS or GT1 (in conjunction with MIB (Measurement Interface Box))
- Heat adhesive for at least 1 hour in cartridge oven (sourcing reference: BMW Parts Service) to 80 +/- 5 °C Write date and time on adhesive when inserting into cartridge oven Insufficient heating (< 1 hour) results in the formation of bubbles/blisters (gluing/cementing not Temperature < 80 +/- 5 °C results in the formation of bubbles/blisters (gluing/cementing not permitted)
- Remove cured adhesive prior to further processing.
- Mistake in mixing in event of an interruption in application >1 minute (gluing/cementing not permitted) A test bead of 50...70 mm must be rejected after an interruption in application
- Best before dates of accelerator and adhesive must not be more than 3 months apart Best before date >3 months results in the formation of bubbles/blisters (gluing/cementing not
Sealed adhesive
- May only be stored for a maximum of 8 hours once it has been heated up to 80 +/- 5 °C.
- The adhesive will be damaged if this time is exceeded (gluing/cementing not permitted)
- Damaged adhesive must not be used and must be disposed of in compliance with national regulations
- Cartridge may only be heated up once If the lower label is black, this adhesive may only still be used cold without accelerator while adhering to the Best before date.
| IMPORTANT | Not all window glass may be bonded with accelerator (hot processing). |
If hot processing is not permitted, this is described in the relevant document.